    威望太小,数据附件不可见,黏贴如下:
    100000    18.92    -3.0117
    69024    19.244    -2.6812
    47644    19.375    -2.6135
    32886    19.629    -2.6426
    22699    19.963    -3.1781
    15668    20.21    -3.7701
    10815    20.539    -4.9346
    7464.9    21.058    -6.4164
    5152.6    21.665    -8.5199
    3556.5    22.464    -11.508
    2454.9    23.595    -15.733
    1694.5    24.886    -21.134
    1169.6    27.088    -28.815
    807.31    29.842    -39.293
    557.24    34.401    -53.096
    384.63    39.157    -73.122
    265.49    46.513    -100.34
    183.25    54.459    -137.41
    126.49    70.067    -183.18
    87.309    99.001    -257.8
    59.71    135.708    -411.22
    40.14    139.77    -403.87
    26.482    201.15    -670.52
    17.117    298.66    -994.81
    10.817    400.21    -1414.1
    6.6698    568.5    -2102.4
    4.0036    877.25    -3293.4
    2.3341    1367    -5104.2
    1.3186    2145.3    -8223.7
    0.72052    4092.7    -16148
    0.38032    5884.2    -23659
    0.19392    10691.5    -42906
    0.09568    18201    -76119
    0.04589    34005    -140200
    0.02154    61043    -257610
    0.01    123640    -497430

0
    +关注 私聊
  • relaxchair

    第2楼2011/04/09

    我也有类似问题,你看看你的nyquest图,然后确定有否wurburg diffusion,考虑修改低频区间,控制电路中的原件或者参数

0
  • 该帖子已被版主-无机麦地加4积分,加2经验;加分理由:感谢您的耐心解答,欢迎常来电化学版块